Consumable manufacturer/ Min yield strength MPa (ksi) 400 (58) 470 (68) 540 (78) 610 (97) 680 (100) 745 (108)
AWS Class ER 7X* ER 8X” ER 9X” ER10X* ER11X” ER12X”
ELGA Elgacore MXA 100, Elgacore MXA 100XP Elgacore MXA 55     Elgacore M690  
ESAB OK Tubrod 14.13, PZ6105R       OK Tubrod 14.03 Coreweld 89
LINCOLN ELECTRIC Outershield MC710-H, Outershield MC715-H          
BÖHLER HL 46-MC, HL 51 T-MC HL53 T-MC, NiCu1 T-MC HL65 T-MC
 
HL75 T-MC alform 700-MC alform 900-MC, alform 960-MC

* X can stand for one or several code characters