SSAB AM Engineering

Download data sheet

General Product Description

SSAB AM Engineering is a gas atomised low-alloyed powder for additive manufacturing of high strength engineering components. SSAB AM Engineering is in particular suited in L-PBF (Laser-Powder Bed Fusion) and Direct Energy Deposition (DED or LMD).

 

The spherical powder enables an optimal combination of strength, toughness and high levels of isotropy in the as-built condition.

 

SSAB AM Engineering is a steel grade with low CO2 emissions, available with SSAB Zero™ steel. SSAB AM Engineering is also planned for fossil-free properties (see www.ssab.com/fossilfree).

Powder Properties

Standard particle size distribution.

L-PBF

20 - 53 µm 1)

DED

53 - 150 µm

1) Max 5% over and under size.

Measurement of particle size distribution is according to ISO 13322-2 (Dynamic image analysis methods).

Other particle size distributions can be arranged upon agreement.

Generic Data

Achievable generic data in as-built parts: L-PBF

Density

7.8 g/cm3

Young´s Modulus

200 GPa

 

Physical Properties

+20 °C
Heat conductivity (W/m*K)
30
Thermal expansion coefficient (10-6/K)
13
+200 °C
Heat conductivity (W/m*K)
34
Thermal expansion coefficient (10-6/K)
15
+400 °C
Heat conductivity (W/m*K)
35
Thermal expansion coefficient (10-6/K)
14

 

Mechanical Properties

Achievable mechanical properties in as-built parts: L-PBF

Product
Product
SSAB AM Engineering
Hardness
(HV5)
340
Tensile strength
(MPa)
1240
Yield strength
(MPa)
1140
Elongation A5
(%)
14
Impact toughness
(Charpy V)
at RT 1)/ at -40 oC
140 J / 47 J

1) At room temperature.

All test samples have been produced on a SLM 280 2.0 system, 30 µm layer thickness and tested in the vertical direction.

Typical Chemical Composition

C
(%)
C
(%)
0.21
Si
(%)
1.03
Mn
(%)
0.72
Cr
(%)
1.04
Mo
(%)
0.20
Fe
Balance

 

Delivery Conditions

Standard package size for SSAB AM powder is 10 kg, including silica gel bag. Other package sizes are available up on agreement.

Safety Information Sheet

SSAB Zero™

SSAB Zero™ is made of recycled steel and produced with fossil-free electricity and biogas. It has virtually no fossil carbon emissions during steel production, without mass balancing allocation of emission reduction or carbon emission offsetting. SSAB Zero™ has the same quality and properties as the traditional steel versions. More details are given in SSAB Zero™ Certificate of Carbon Emissions at www.ssab.com.