SSAB Docol® Automotive Steel Grades

Maximize your choice of AHSS/UHSS automotive solutions: SSAB Docol® automotive steel grades include martensitic • press hardening steel • complex phase • high edge ductility • 3rd gen dual phase with high formability • and more. SSAB uses pure Swedish iron ore and advanced milling processes to make steels with extremely clean properties and highly consistent formability.

OEM-specific automotive steels

In addition to the automotive steel grades listed below, SSAB offers hundreds of SSAB Docol® variations to meet specific VDA, SAE, EN, JIS, and OEM standards. We work in close cooperation with automotive OEMs and Tier 1 suppliers to develop custom AHSS grades that give your designs a competitive edge.

 

Custom AHSS for automotive OEMs
Body in white

Resources for each phase of development

We can help at each step: material selection, crash simulations, design optimization, production modeling, effective workflow planning, and tooling recommendations. Plus, you have immediate access to on-demand webinars and articles on key issues such as AHSS simulations, managing springback, and fossil-free automotive steel.

SSAB Docol resources

The newest AHSS grades

In addition to the open for sales steels listed in the “Available steel grades” tables below, SSAB is constantly developing new SSAB Docol® grades based on future needs of leading car OEMs and Tier 1 suppliers.

Here’s a list of exciting new AHSS developments. Some are “steel family extensions” — that is, grades now available in new hot-rolled or metal-coated versions. Others are all-new automotive metals, like our guaranteed hole-expansion ratio (HER) grades.

New hot-rolled grades:

SSAB Docol HR800HER-75
SSAB Docol HR800HER-100
SSAB Docol HR1500M
SSAB Docol HR1000CP

New cold-rolled grades:

SSAB Docol 1900M
SSAB Docol 1700M-EG

New metal-coated grades:

SSAB Docol CR1180CP-GI
SSAB Docol CR1180DP-GI
SSAB Docol CR1000DH-GI
SSAB Docol HR600FB-GI

Available steel grades

Martensitic (M) steels

Martensitic (M) steels have very high yield strength (Re) and an extremely high tensile strength (Rm). SSAB Docol® martensitic steel has good draw ability and good edge stretching properties. It is also good in welding.

SSAB Docol® Martensitic phase steel product offer:

Product Family

SSAB Docol 900M

Product Name
Docol CR​700Y​900T-​MS
Coating
UC, EG
Dimensions
T: 0.50 - 2.10 mm
W: Up to 1527 mm
T: 0.020 - 0.0827 in
W: Up to 60.12 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 1100M

Product Name
Docol CR​860Y​1100T-​MS
Coating
UC, EG
Dimensions
T: 0.50 - 2.00 mm
W: Up to 1527 mm
T: 0.020 - 0.0787 in
W: Up to 60.12 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 1200M

Product Family

SSAB Docol 1300M

Product Name
Docol CR​1030Y​1300T-​MS
Coating
UC, EG
Dimensions
T: 0.50 - 2.10 mm
W: Up to 1527 mm
T: 0.020 - 0.0827 in
W: Up to 60.12 in
Standards
VDA 239-100
Datasheet
Product Family

SSAB Docol 1400M

Product Name
Docol CR​1150Y​1400T-​MS
Coating
UC, EG
Dimensions
T: 0.50 - 2.10 mm
W: Up to 1527 mm
T: 0.020 - 0.0827 in
W: Up to 60.12 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 1700M

Product Name
Docol CR​1350Y​1700T-​MS
Coating
UC
Dimensions
T: 1.00 - 2.10 mm
W: Up to 1250 mm
T: 0.0394 - 0.0827 in
W: Up to 49.21 in
Standards
VDA 239-100
Datasheet

*Available upon request.

Dual phase with high formability

Metal coated SSAB Docol® 600DH-GI and 800DH-GI are two of the steel grades now avaliable and more are on the way.

DA special heat treatment producing mainly two-phase structure makes SSAB Docol® 600DH-GI and 800DH-GI suitable where an improved formability is requested compared to conventional dual-phase steel grades with the same tensile strength level.

Product Family

SSAB Docol 600DH

Product Name
Docol CR​330Y​590T-​DH
Coating
GI
Dimensions
T: 0.80 - 2.40 mm
W: Up to 1400 mm
T: 0.031 - 0.0945 in
W: Up to 55.12 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 800DH

Product Name
Docol CR​440Y​780T-​DH
Coating
GI
Dimensions
T: 0.80 - 2.00 mm
W: Up to 1400 mm
T: 0.031 - 0.0787 in
W: Up to 55.12 in
Standards
VDA 239-100
Datasheet

Press Hardening Steel (PHS)

For Press Hardening (PHS) Steel it is the forming process which sets the final characteristics on the material. Forming at high temperatures facilitates complex structures as the martensitic microstructure is developed after press hardening. This material has a limitation in welding properties.

SSAB Docol® PHS steel product offer:

Product Family

SSAB Docol PHS 1800

Product Name
Docol PHS FH 1800
Coating
UC
Dimensions
T: 0.70 - 3.00 mm
W: Up to 1500 mm
T: 0.028 - 0.118 in
W: Up to 59.06 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol PHS 1500

Complex Phase (CP) steels

Complex Phase (CP) steels have higher yield strength and lower work hardening effect, compared to DP steels for same strength level. The CP steels have good fatigue properties when it comes to low cycle fatigue. Compared to DP, the CP steels offer better flanging and ISO hole expansion performance and these automotive metals are suitable for applications where high strength, good bendability and stretch-flange ability is required.

SSAB Docol® Complex phase steel product offer:
Product Family

SSAB Docol 600CP

Product Name
Docol CR​350Y​600T-​CP
Coating
GI, GA, ZA
Dimensions
T: 0.70 - 2.50 mm
W: Up to 1520 mm
T: 0.028 - 0.0984 in
W: Up to 59.84 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 800CP

Product Family

SSAB Docol 1200CP

Product Name
Docol CR​900Y​1180T-​CP
Coating
UC, EG, GI*
Dimensions
T: 0.50 - 2.10 mm
W: Up to 1527 mm
T: 0.020 - 0.0827 in
W: Up to 60.12 in
Standards
VDA 239-100
Datasheet

*Available upon request.

Dual Phase (DP) steels

For Dual Phase (DP) steels there is a big difference in yield and tensile strength in un-deformed areas. The work hardening in forming is very strong. DP steels have good formability compared to its strength but are limited in hole expansion. With its lean composition these steels are easy to weld but sensitive to heat treatment (> 200 °C).

SSAB Docol® dual phase steel product offer:

Product Family

SSAB Docol 500DP

Product Family

SSAB Docol 800DP

Product Family

SSAB Docol 1000DP

*Available upon request.

High Edge Ductility steel for Cars

SSAB Docol® HE is a new range of hot rolled advanced high strength steel (AHSS) with improved edge ductility for automotive manufacturers facing technical challenges in production.

SSAB Docol® High Edge Ductility steel product offer:

Product Family

SSAB Docol 355HE

Product Name
Docol HR355Y430T HE
Coating
UC
Dimensions
T: 2.00 - 7.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.276 in
W: Up to 62.99 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 420HE

Product Name
Docol HR420Y480T HE
Coating
UC
Dimensions
T: 2.00 - 7.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.276 in
W: Up to 62.99 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 460HE

Product Name
Docol HR460Y520T HE
Coating
UC
Dimensions
T: 2.00 - 7.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.276 in
W: Up to 62.99 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 500HE

Product Name
Docol HR500Y550T HE
Coating
UC
Dimensions
T: 2.00 - 7.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.276 in
W: Up to 62.99 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 550HE

Product Name
Docol HR550Y600T HE
Coating
UC
Dimensions
T: 2.00 - 7.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.276 in
W: Up to 62.99 in
Standards
SSAB
Datasheet

High Strength Low Alloy (HSLA) steels 

High Strength Low Alloy (HSLA) steels have a typically small difference between yield strength and tensile strength (<100 MPa). They, therefore, offer excellent bendability. With little pearlite and no other hard phases they also have better fine blanking properties compared to DP steels and due to lean composition they are very easy to weld.

SSAB Docol® High Strength Low Alloy steel product offer:

Product Family

SSAB Docol S600MC

Product Family

SSAB Docol 500LA

Product Family

SSAB Docol 420LA

Product Family

SSAB Docol 550LA

Product Name
Docol HR​550LA
Coating
UC, GI*
Dimensions
T: 2.00 - 6.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.236 in
W: Up to 62.99 in
Standards
VDA 239-100
Datasheet
Product Family

SSAB Docol 600LA

Product Name
Docol HR​600LA
Coating
UC
Dimensions
T: 2.00 - 6.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.236 in
W: Up to 62.99 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 650LA

Product Name
Docol HR​650LA
Coating
UC
Dimensions
T: 2.000 - 6.00 mm
W: Up to 1600 mm
T: 0.07874 - 0.236 in
W: Up to 62.99 in
Standards
SSAB
Datasheet
Product Family

SSAB Docol 700LA

Product Name
Docol HR​700LA
Coating
UC, EG, GI*
Dimensions
T: 2.00 - 6.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.236 in
W: Up to 62.99 in
Standards
VDA 239-100
Datasheet
Product Family

SSAB Docol S900MC

Product Name
Docol S900MC
Coating
-
Dimensions
T: 3.00 - 10.00 mmT: 0.118 - 0.3937 in
Standards
EN 10149-2
Datasheet
Product Family

SSAB Docol S960MC

Product Name
Docol S960MC
Coating
-
Dimensions
T: 3.00 - 10.00 mmT: 0.118 - 0.3937 in
Standards
EN 10149-2
Datasheet
Product Family

SSAB Docol HR100XF

Product Name
Docol HR100XF
Coating
UC
Dimensions
T: 2.00 - 10.00 mmT: 0.079 - 0.393 in
Standards
-
Datasheet
Product Family

SSAB Docol HR110XF

Product Name
Docol HR110XF
Coating
UC
Dimensions
T: 2.00 - 10.00 mmT: 0.079 - 0.393 in
Standards
-
Datasheet

*Available upon request.

Ferritic-Bainitic

Ferritic-Bainitic (FB) steels have mechanical properties that are similar to Complex Phase (CP) steels but with a higher gap between yield and tensile strength. FB steels are characterized by good bendability and excellent stretch-flange ability. They are best suited for parts with stretched flanges such as chassis components in cars.

Product Family

SSAB Docol 600FB

Product Name
Docol HR​440Y​580T-​FB
Coating
UC, GI*
Dimensions
T: 2.00 - 4.00 mm
W: Up to 1600 mm
T: 0.0787 - 0.157 in
W: Up to 62.99 in
Standards
VDA 239-100
Datasheet

*Available upon request.

Tubes

SSAB Docol Tubes offer the market´s greatest strength range. The tensile strength range starts from 600 MPa and goes up to an extraordinary 1000 MPa without any post-heat treatments. With coating options including zinc, galfan and galvannealed, corrosion resistance and superior paint adhesion can be combined for the first time in high-strength precision tubing. SSAB Docol Tubes are made in compliance with standard EN 10305 (parts 3 and 5) with the more demanding elongation values and chemical analyses. To meet the highest customer expectations, we manufacture the tubes with narrow tolerances.

Product Family

SSAB Docol Tube 590DP

Product Family

SSAB Docol Tube 980DP

Product Name
CR750Y980T-DP
Dimensions
Circular: 28.0 - 60.0 mm
Square: 25x25 - 50x50 mm
Rectangular: 40x20 - 60x40 mm
Wall Thickness: 1.0 - 2.0 mm
Circular: 1.10 - 2.36 in
Square: in
Rectangular: in
Wall Thickness: 0.039 - 0.079 in
Standards
EN 10305-3, VDA 239-100
Datasheet
Product Family

SSAB Docol Tube 600LA

Product Name
HR600LA
Dimensions
Circular: 22.0 - 88.9 mm
Square: 30x30 - 60x60, 30x30 - 60x60 mm
Rectangular: 30x20 - 100x40 mm
Wall Thickness: 2.0 - 3.0 mm
Circular: 0.866 - 3.50 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.12 in
Standards
EN 10305-3
Datasheet
Product Family

SSAB Docol Tube 700LA

Product Name
HR700LA
Dimensions
Circular: 32.0 - 88.9 mm
Wall Thickness: 2.0 - 3.0 mm
Circular: 1.26 - 3.50 in
Wall Thickness: 0.079 - 0.12 in
Standards
EN 10305-3
Datasheet
Product Family

SSAB Docol Tube R8

Product Name
Docol Tube R8
Dimensions
Circular: 25.4 - 50.8 mm
Wall Thickness: 1.24 - 2.4 mm
Circular: 1.00 - 2.00 in
Wall Thickness: 0.0488 - 0.095 in
Standards
EN 10305-3
Datasheet