SSAB Boron Tube 24 is a structural hollow section for hardening. It offers good workshop properties in delivery condition. The degree of hardness and toughness that can be achieved after heat-treatment will provide the final products with wear- and shock resistance properties that assure longer lifetime.
SSAB Boron Tube 24 is available at circular.
Other shapes, sizes and lengths are available upon request.
Typical mechanical properties when quenched to water:
Rp0.2 ~1100 MPa; Rm ~1400 MPa; A~8%