Armox® 560T

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

On this page

General Product Description

High hardness armor with extraordinary toughness properties.

Armox® 560T is the world’s toughest protection plate, having nominal 560 HBW hardness, for use in vehicles, buildings and many more applications.

Benefits of Armox® 560T include: 

  • Market-leading steel protection
  • Superior workshop properties
  • Optimized solutions
  • Perfect hardness/toughness balance, for combined penetration and blast protection
  • Expertise in ballistic protection from SSAB

It offers vehicle designers new ways to increase protection using lighter weight designs.

Armox® 560T is not intended for further heat treatment.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Thickness
    (mmin)
    Hardness
    (HBW)
    Yield strength Rp0.2
    (min MPaksi)
    Tensile strength Rm
    (MPaksi)
    Elongation A5
    (min %)
    Elongation A50
    (min %)
    4.0 - 15.00.157 - 0.591 530 - 590 1300188 1650 - 2000239 - 290 7 9
    Compare parameters

    Select one parameter to compare

    Comparison

       

      Mechanical Testing

      Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual.

      Charpy impact test according to EN ISO 148 on each heat and thickness from 6 mm.

      Tensile test according to EN ISO 6892 on each heat.

      Ultrasonic testing

      According to EN ISO 10160 Class E3S3.

      Impact Properties

      Hide/Show specific columns Edit
      Select columns to display
        Thickness
        (mmin)
        Min impact energy for transversal testing,
        Charpy V 10x10 mm test specimen 1)
        4.0 - 15.00.157 - 0.591 20 J / -40 °C15 ft-lbs / -40 °F
        Compare parameters

        Select one parameter to compare

        Comparison

          Thickness
          (mmin)
          4.0 - 15.00.157 - 0.591
          Min impact energy for transversal testing,
          Charpy V 10x10 mm test specimen 1)
          20 J / -40 °C15 ft-lbs / -40 °F

          1) Average of three tests. Transverse to rolling direction. Single value min. 70% of specified average. For plate thicknesses under 12 mm sub-size Charpy-V specimen are used. The specified minimum value is then propotional to the specimen cross-section.

          Chemical Composition (ladle analysis)

          Hide/Show specific columns Edit
          Select columns to display
            C *)
            (max %)
            Si *)
            (max %)
            Mn*)
            (max %)
            P
            (max %)
            S
            (max %)
            Cr*)
            (max %)
            Ni*)
            (max %)
            Mo*)
            (max %)
            B*)
            (max %)
            0.37 0.70 1.00 0.010 0.003 1.0 1.80 0.50 0.005
            Compare parameters

            Select one parameter to compare

            Comparison

              The steel is grain-refined. *) Intentional alloying elements.

              Tolerances

              More details are given in SSAB brochure Armox® Guarantees or on www.ssab.com.

              Thickness

              Tolerances according to Armox® Thickness Guarantees.

              Armox® Guarantees meet the requirements of EN 10029 Class C, but offers narrower tolerances.

              Length and Width

              Tolerances conform to EN 10029 or to SSAB´s standard after agreement.

              Dimensional tolerances for plate with mill edge according to special agreement. 

              Shape

              Tolerances according to EN 10029.

              Flatness

              Tolerances according to Armox® flatness guarantees, which are more restrictive than EN 10029 Class N (steel type L).

              Surface Properties

              According to EN 10163-2 Class B, Subclass 3.

              Delivery Conditions

              The delivery condition is QT (Quenched and Tempered).

              Delivery requirements can be found in SSAB’s brochure Armox® Guarantees or www.ssab.com.