Weathering steel in the grades and shapes you need
The SSAB Weathering portfolio includes a wide range of heavy plate, hot and cold rolled strip, tube and sections with yield strength from 345 to 960 MPa.
The SSAB Weathering portfolio includes a wide range of heavy plate, hot and cold rolled strip, tube and sections with yield strength from 345 to 960 MPa.
Weather-resistant steel from SSAB is easy to work with and give your products and installations the long-term performance you are looking for.
SSAB Weathering has excellent properties for forming, machining and welding. The SSAB Weathering portfolio includes a wide range of grades with mechanical properties and dimensional tolerances that generally exceed the standards given by EN 10025-5, and ASTM grades.
SSAB Weathering steel grades are available from stock or mill. You can also order a trial delivery for testing in your production.
Your local service contact will answer any questions about ordering and shipping, delivery times, marking and packing.
Product Name | Dimensions | Standards | Datasheet |
---|---|---|---|
SSAB Weathering 355 |
T: 0.50 - 12.00 mm W: Up to 1860 mmT: 0.020 - 0.4724 in W: Up to 73.23 in |
SSAB | |
SSAB Weathering 420 |
T: 3.0 - 12.0 mm W: Up to 1860 mmT: 0.12 - 0.472 in W: Up to 73.23 in |
EN 10025-5 | |
SSAB Weathering 460 |
T: 3.0 - 12.0 mm W: Up to 1800 mmT: 0.12 - 0.472 in W: Up to 70.87 in |
EN 10025-5 | |
SSAB Weathering 550 |
T: 3.00 - 12.00 mm W: Up to 1550 mmT: 0.118 - 0.4724 in W: Up to 61.02 in |
SSAB | |
SSAB Weathering 355NL | T: 5.00 - 100.00 mmT: 0.197 - 3.9370 in | EN 10025-5 | |
SSAB Weathering 355ML | T: 8.00 - 65.00 mmT: 0.315 - 2.559 in | EN 10025-5 | |
SSAB Weathering 420ML | T: 8.00 - 65.00 mmT: 0.315 - 2.559 in | EN 10025-5 | |
SSAB Weathering 460ML | T: 8.00 - 65.00 mmT: 0.315 - 2.559 in | EN 10025-5 |
Product Name | Dimensions | Standards | Datasheet |
---|---|---|---|
SSAB Weathering Tube 355WH |
Circular: 42.4 - 323.9 mm Square: 40x40 - 300x300 mm Rectangular: 50x30 - 400x200 mm Wall Thickness: 2.0 - 12.5 mmCircular: 1.67 - 12.75 in Square: in Rectangular: in Wall Thickness: 0.079 - 0.492 in |
EN 10219-2, EN 1090-2 | |
SSAB Weathering Tube 500WH |
Circular: 42.4 - 323.9 mm Square: 40x40 - 300x300 mm Rectangular: 50x30 - 400x200 mm Wall Thickness: 2.0 - 12.5 mmCircular: 1.67 - 12.75 in Square: in Rectangular: in Wall Thickness: 0.079 - 0.492 in |
EN 10219-2 |