Combines ballistic properties with impact toughness.
Ramor® 450 is a medium-hard protection plate combining ballistic properties with impact toughness, at 8.0 ‑ 16.0 mm (0.315‑0.630″) thick and 400‑480 HBW. Ramor® 450 is not intended for further heat treatment.
Ramor® 450
Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual/coil.
Hardness is measured on a milled surface 0.3 - 2.0 mm below plate surface.
Charpy impact test according to EN ISO 148, 1 test/20 ton.
Tensile test according to EN ISO 6892 on each plate and thickness <19.9 mm.
1) Impact testing transverse to rolling direction, average value of three tests. Single value min. 70% of specified average.
The steel is grain refined. Phosphorous and sulphur are not intentionally alloying elements.
More details are given on www.ssab.com.
Tolerances conform to EN 10029 or to SSAB´s standard after agreement.
Dimensional tolerances for plate with mill edge according to special agreement.
Tolerances according to EN 10029.
Tolerances according to SSAB’s flatness tolerances which are more restrictive than EN 10029 Class N (steel type L).
According to EN 10163-2 Class B, Subclass 3.
Ramor® is delivered in quenched condition.