Ramor® SR500 is a ballistic steel well suited for shooting ranges, shooting targets etc.
Ramor® SR500 is available as plate in thicknesses of 4.8 - 12.7 mm (0.188 - 0.500").
Dimensions upon agreement.
Product | Hardness (HBN) |
|---|---|
Ramor® SR500 | 500 - 590 |
C (max %) | Mn (max %) | Si (max %) | Cr (max %) | CE(IIW) Typical |
|---|---|---|---|---|
0.32 | 1.6 | 0.7 | 2.0 | 0.7 |
Thickness, width and length tolerances are in accordance with ASTM A6.
Flatness tolerances according to ASTM A6.
Plates are delivered in quenched or quenched and tempered condition.