SSAB Steel Service Center in Oborniki, Poland has a wide range of steel processing capabilities. From shot blasting and cutting to bending, drilling, machining and much more.

If requested, we can shot blast each plate entering our facility, to ensure premium Surface condition of each part. We use Schlick shot blasting line with following parameters:
PLATE THICKNESS RANGE: 6–200 mm
PLATE WIDTH: 2500 mm
PLATE MAXIMUM WEIGHT: 10 000 kg
ABRASIVE MEDIUM: Steel, Sa 2.5

Depending on the part specification, plate thickness and customers’ requirements, we can use the following thermal cutting methods in our facility.
MANUFACTURER: Messer
TABLE SIZE: 2500x13000 mm
NO OF TORCHES: 4
BEVELIING: flame or mechanical
TOLERANCES: EN 9013-1 Class 2
MANUFACTURER: Messer
TABLE SIZE: 5000x13000 mm
NO OF TORCHES: 12
BEVELIING: flame or mechanical
TOLERANCES: EN 9013-1 Class 2

Depending on the part specification, plate thickness and customers’ requirements we can use the following thermal cutting methods in our facility.
MANUFACTURER: ESAB
TABLE SIZE: 3000x14000mm
PLASMA TORCH: 3D torch 540 , cuting angle up to 45
PLASMA SOURCE: ESAB 450A
OXY-GEN TORCHES: 2
TOLERANCES: EN 9013-1 Class 2
MANUFACTURER: Messer
TABLE SIZE: 2500x13000mm
NO OF TORCHES: 2
PLASMA SOURCE: Hypertherm 260A
TOLERANCES: EN 9013-1 Class 2
MANUFACTURER: Messer
TABLE SIZE: 5000x13000mm
NO OF TORCHES: 2
PLASMA SOURCE: Hypertherm 260A
TOLERANCES: EN 9013-1 Class 2

Depending on the part specification, plate thickness and customers’ requirements, we can use the following thermal cutting methods in our facility.
MANUFACTURER: Messer
TABLE SIZE: 4100x14000 mm
LASER: Fanuc CO2 6 kw, 3D endless rotating bevel head
TOLERANCES: EN 9013-1 Class 1

Depending on the part specification, plate thickness and customers’ requirements, we can use one of the following press brakes:
MANUFACTURER: Ursviken
BENDING LENGTH: 12200 mm
DISTANCE BETWEEN COLUMNS: 10200 mm
MAXIMUM PRESS POWER: 2000 ton
VARIABLE DIE SCOPE: 40-300 mm
Flexicrown – precise deflection control
Ecopump – Energy saving ecological pump
6-axis CNC controlled back gauge
MANUFACTURER: Durma
BENDING LENGTH: 10500 mm
DISTANCE BETWEEN COLUMNS: 9000 mm
MAXIMUM PRESS POWER: 1500 ton
MANUFACTURER: Aliko
BENDING LENGTH: 4000 mm
MAXIMUM PRESS POWER: 400 ton

Depending on specific needs and requirements, we can provide further precise processing, such as:
Drilling with Pax radial drilling machine, which we use for drilling, threading, counterboring and other operations in mild
steels, high-strength steels and Hardox® wear plate.
We also process parts with mechanical chamfering and grinding for edge preparation.

In addition to premium products, we also offers a number of services to facilitate your product development. Contact us to see what we can do for you.