Want to discover unique automotive applications for AHSS materials? Try new production methods? Or create lighter components that can improve fuel efficiency, crash-worthiness and sustainability?
The SSAB Trial Material Stock Center is a unique service in the steel industry: We deliver AHSS/UHSS sheets, coils and custom lengths, even in letter size, to nearly anywhere in the world. In 1 to 2 weeks, your Docol® AHSS/UHSS samples are ready for dispatch. Our stocking program gives you quick access to AHSS trial materials, so you can work it, test it, inspect it, try out new production methods, and accelerate your time to market.
The Docol material stock program includes cold-rolled, cold-rolled electrogalvanized, metal-coated and hot-rolled pickled AHSS/UHSS steel grades. Sheets range from A4 (letter size) to 4 meters (13.1 feet). Slit AHSS trial samples come in widths of 9 mm and higher, and coils range from one metric ton to full size.
We supply many AHSS/UHSS steel grades, including many made to VDA and OEM standards.

High-Strength Low Alloy (HSLA):
Docol 420–500LA, 0.80–3.00 mm
Dual Phase (DP):
Docol 500–1180DP, 0.80–2.00 mm
Martensitic (M):
Docol 1100–1700M, 0.80–2.00 mm
Electrogalvanized Martensitic (M), 7.5 micron zinc layer double sided:
Docol 1300, 1500, 1700M-EG, 1.00–2.00 mm
Roll-forming:
Docol Roll 800–1000, 0.80–2.00 mm
Press-hardening:
Docol PHS 2000, 1.00–3.00 mm
Complex Phase (CP):
Docol PHS CR 2000, 1.00–3.00 mm
High-Strength Low Alloy (HSLA) acc. to VDA:
Docol HR 700LA, 2.00–2.50 mm
Dual Phase (DP) acc. to VDA:
Docol 590–980DP, 0.80–2.00 mm
Complex Phase (CP) acc. to VDA:
Docol 780-1180CP, 1.00–2.00 mm
Docol HR660Y760T-CP, 2.00–2.50 mm
Dual Phase with High Ductility steels acc. to VDA:
Docol 590–1000DH, 1.20–1.80 mm
Ferrite Bainite (FB) acc. to VDA:
Docol HR440Y580T-FB, 2.50–3.00 mm
High-Strength Low Alloy (HSLA):
Docol HR 700LA, 2.00–3.00 mm
High Edge Ductility (HE):
Docol HR355Y430T HE, 2.00–4.00 mm
Docol HR420Y480T HE, 2.00–4.00 mm
Docol HR460Y520T HE, 2.00–4.00 mm
Docol HR500Y550T HE, 2.00–4.00 mm
Complex Phase (CP):
Docol HR 800CP, 2.00–4.00 mm
Docol HR 800HER-75, 2.00–4.00 mm
Docol HR 800HER-100, 2.00–4.00 mm
Docol HR800Y950T-CP, 2.50–3.00 mm
Martensitic (M):
Docol HR 1200M, 2.00–3.00 mm
Docol HR 1500M, 2.00–3.00 mm
Ferrite Bainite (FB):
Docol 440Y580T-FB, 2.50–4.00 mm
In addition to the electrogalvanized grades listed here, SSAB also offers galvannealed and Galfan® samples upon request. We can also provide sample AHSS tubes in a variety of dimensions. For more information please contact your Docol automotive steel expert.
New Docol AHSS/UHSS samples are constantly being added to our trial stock program. Our technical specialists can help you decide which AHSS/UHSS steel grade and thickness should be used in a specific application, as well as provide forming data and other detailed technical information.