Strenx® 1100 is a group of structural steel grades with a minimum yield strength of 1100 MPa (160 ksi). Excellent for advanced lifting devices.
SUITABLE APPLICATIONS
Advanced lifting devices and lighter transport solutions
TYPE OF PRODUCTS
Hot rolled strip, Plate, Cold rolled strip
THICKNESS RANGE
0,8 - 40 mm (0.031’’ – 1.57’’)
STRENX® 1100 E
Superior toughness
Made for advanced lifting devices, such as mobile cranes, and lighter transport solutions and components
Impact toughness: 27 J/-40°C (20 ft-lb/-40°F)
Plate: 4-40 mm (0.157’’ – 1.57’’)
Standard: SSAB specification
Format: Plate
STRENX® 1100 F
Extreme toughness
Made for advanced lifting devices, such as mobile cranes, and lighter transport solutions and components in cold conditions
Impact toughness: 27 J/-60°C (20 ft-lb/-76°F)
Plate: 4-40 mm (0.157’’ – 1.57’’)
Standard: SSAB specification
Format: Plate
STRENX® 1100MC
Multipurpose cut-to-length sheets
Load-bearing structures, where strength and weight is critical
Impact toughness: 27 J/-40°C (20 ft-lb/-40°F)
Hot rolled strip: 3-8 mm (0.118’’ – 0.393’’)
Standard: SSAB specification
Format: Sheet
STRENX® 1100 CR
For the thinnest structural parts
A wide range of components and parts in the lightest possible load-bearing structures
Cold rolled strip: 0.8-2.1 mm (0.032’’ –0.082”)
Standard: SSAB specification
Format: Sheet

Mobile cranes, loader cranes, work platforms and other lifting equipment can achieve new levels of performance by using Strenx® 1100 high-strength structural steel. Optimizing the design to take advantage of the high strength makes the equipment lighter, giving increased load capacity and longer reach. For support on designing with Strenx® 1100, get in touch with SSAB Tech Support.
Contact tech support
Strenx® 1100 can be welded using any conventional welding method. MAG welding is the most common technique today, since it is very easy to automate for high productivity.

Strenx® 1100 can usually be machined without special equipment. Stable machinery fitted with high-speed steel and carbide tools is recommended when drilling, countersinking, tapping, turning, and milling.

Free bending and roll bending of Strenx® steel plate and strip can be done using standard bending machinery. Uniform properties, close thickness tolerances and high surface quality ensure a predictable bending process.

The properties and fine surface finish of Strenx®1100 plate and strip makes it perfect for laser cutting. Thermal cutting of hot-rolled Strenx® 1100 steel sheet and plate is performed with oxy-fuel flame, plasma and laser.

Mechanical cutting of Strenx® 1100 is best performed with guillotine shears. Consider carefully the settings of the cutting machine. The most important factors are clearance, cutting angle and blade hardness. The plate should be allowed to warm up thoroughly to around +20°C before it is cut.

Strenx® guarantees include tight thickness tolerances, tight flatness tolerances and bending guarantees. The tight thickness tolerances enable you to know the weight more precisely. As a result, you can reduce your safety margins. Precise thickness within a plate and between plates makes for safe and predictable performance in the workshop.
Learn more about your guaranteesTension bars in Strenx® 1100 E a safe choice in XCMG’s record-breaking crawler cranes.
Read the full story
| Strenx® 1100 standard products | Thickness range [mm] | Confirm to standard | Formats | Typical products manufactured with Strenx® | ||
|---|---|---|---|---|---|---|
| Plate | Hot rolled strip | Cold rolled strip | ||||
| Strenx® 1100 E | 4-40 | --- | --- | SSAB specification | Plates | Advanced lifting devices, such as mobile cranes, and lighter transport solutions and components |
| Strenx® 1100 F | 4-40 | --- | --- | SSAB specification | Plates | Advanced lifting devices, such as mobile cranes, and lighter transport solutions and components in cold conditions |
| Strenx® 1100 MC | --- | 3-8 | --- | SSAB specification | Sheets | Load-bearing structures, where strength and weight is critical |
| Strenx® 1100 CR | --- | --- | 0.8-2.1 | SSAB specification | Sheets & Coils | A wide range of components and parts in the lightest possible load-bearing structures |