At the Steel Service Center in Ghedi, steel processing is carried out by highly skilled personnel, with rigorous checks at every stage of the process.
Our Cut to Length line can transform HR steel grades with a yield strength of up to 700 MPa, accommodating thicknesses up to 16 mm and widths up to 2000 mm.
Additionally, through an integrated system of subcontractors, we also provide services such as pickling, slitting, shear blanking, and processing of cold-rolled and metal-coated cut to length.
Cutting capability


In addition to premium products, we also offer a number of services to facilitate your product development. Contact us to see what we can do for you.