High hardness armor with extraordinary toughness properties.
Armox® 500T is the world’s toughest protection plate, having nominal 500 HBW hardness, for use in vehicles, buildings and many more applications.
Benefits of Armox® 500T include:
It offers vehicle designers new ways to increase protection using lighter weight designs.
Armox® 500T is not intended for further heat treatment.
Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual.
Charpy impact test according to EN ISO 148-1 on each heat and thickness from 6 mm.
Tensile test according to EN ISO 6892-1 on each heat and thicknesses.
According to EN 10160 Class E3S3 for thicknesses up to 80 mm and E1S2 for > 80 mm.
1) Average of three tests. Transverse to rolling direction. Single value min. 70% of specified average. For plate thicknesses under 12 mm sub-size Charpy-V specimen are used. The specified minimum value is then propotional to the specimen cross-section.
1) For plate thicknesses >70 mm Cr ≤ 1.5 and Ni ≤3.5.
The steel is grain-refined. *) Intentional alloying elements.
Tolerances according to Armox® Thickness Guarantees.
Armox® Guarantees meet the requirements of EN 10029 Class C, but offers narrower tolerances.
Tolerances conform to EN 10029 or to SSAB´s standard after agreement.
Dimensional tolerances for plate with mill edge according to special agreement.
Tolerances according to EN 10029.
Tolerances according to Armox® flatness guarantees, which are more restrictive than EN 10029 Class N (steel type L).
According to EN 10163-2 Class B, Subclass 3.
The delivery condition is QT (Quenched and Tempered). Plates with thicknesses over 50 mm are delivered with mill edge as standard.