Product offer and datasheets

Toolox® engineering and tool steel meets and exceeds the demands of state-of-the-art industrial production equipment. It is produced to exacting chemical and mechanical properties that outperform traditional steel grades in regard to cleanliness, consistency, hardness and toughness, machinability and other vital parameters for fast production and reliable performance of the final products.

Show specs in:

MetricImperial

Introducing Toolox® 46 with higher heat resistance

We have tweaked the alloying recipe and created Toolox® 46 with improved performance in hot work tooling applications. It has a hardness of 430-490 HBW and the same easy machining properties as other Toolox® products. Get in touch if you like to try it!

Product Name

Toolox® 46

Hardness (HBW)
430 - 490
Dimensions (mmin)
T: 60.0 - 320.0
D: 151.0 - 353.0
T: 2.36 - 12.60
D: 5.945 - 13.898
Min. Impact Toughness
11 J / 20 °C8 ft-lbs / 68 °F
Standards
EN 10029, EN 10060
Datasheet

Toolox® 44

Toolox® 44 is a prehardened steel highly suitable forhigh-performing machine part and tooling of all sizes and shapes. The steel’s cleanliness, low carbide content and vibration dampening properties all work together to provide excellent machinability and reduced wear on tool inserts even in the fastest and most powerful CNC machines.

Product Name

Toolox® 44

Hardness (HBW)
410 - 475
Dimensions (mmin)
T: 6.0 - 320.0
D: 21.0 - 353.0
T: 0.236 - 12.598
D: 0.827 - 13.898
Min. Impact Toughness
11 J / 20 °C6 ft-lbs / 68 °F
Standards
EN 10029, EN 10060
Datasheet

Toolox® 33

Toolox® 33 is used in a wide variety of machine components and tooling. The steel will not deform even after extensive machining to create complex shapes. It’s has equal hardness throughout the material and high impact toughness for reliable usage under the most demanding conditions The low carbon and alloy content make hot cutting suitable. Giving the possibility to cut closer to final shape before machining.

Product Name

Toolox® 33

Hardness (HBW)
275 - 325
Dimensions (mmin)
T: 6.0 - 130.0T: 0.236 - 5.118
Min. Impact Toughness
35 J / 20 °C26 ft-lbs / 68 °F
Standards
EN 10029
Datasheet
Product Name

Toolox® 40

Hardness (HBW)
360 - 420
Dimensions (mmin)
T: 6.0 - 130.0T: 0.236 - 5.118
Min. Impact Toughness
20 J / 20 °C15 ft-lbs / 68 °F
Standards
EN 10029
Datasheet