Extra-high-hardness armor with very good resistance against penetration.
Armox® 600T is used as an add-on protection plate or where weight is critical. Armox® 600T is available in thicknesses between 4 and 20 mm with a guaranteed hardness range of 570‑640 HBW.
Benefits of Armox® 600T include:
Armox® 600T is not intended for further heat treatment.
Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual.
Charpy impact test according to EN ISO 148 on each heat and thickness from 6 mm.
According to EN 10160 Class E3S3.
1) Average of three tests. Transverse to rolling direction. Single value min. 70% of specified average. For plate thicknesses under 12 mm sub-size Charpy-V specimen are used. The specified minimum value is then propotional to the specimen cross-section.
The steel is grain-refined. *) Intentional alloying elements.
Tolerances according to Armox® Thickness Guarantees.
Armox® Guarantees meet the requirements of EN 10029 Class C, but offers narrower tolerances.
Tolerances conform to EN 10029 or to SSAB´s standard after agreement.
Dimensional tolerances for plate with mill edge according to special agreement.
Tolerances according to EN 10029.
Tolerances according to Armox® flatness guarantees, which are more restrictive than EN 10029 Class N (steel type L).
According to EN 10163-2 Class B, Subclass 3.
The delivery condition is QT (Quenched and Tempered).
Delivery requirements can be found in SSAB’s brochure Armox® Guarantees or www.ssab.com.