SSAB Weathering steel, compliant with the EN 10219 and the EN 10025-5 standards, provides a more sustainable, long-lasting corrosion resistance for telecommunication towers, power transmission towers, and electric utility poles.
With no galvanizing or painting required – ever – SSAB Weathering steel delivers a more sustainable corrosion resistance solution for your towers and utility poles. SSAB Weathering steel lowers CO2 emissions throughout the production process, as well as during service by eliminating the need to recoat. Unlike galvanized steel, there is no zinc run-off and the patina color blends in well in both natural and city settings.


Galvanizing 8mm thick steel with an 85-micron (μm) coating can add 120 kg CO2e to every tonne, before factoring in added transportation to galvanizing facilities. To further reduce CO2e, check out our steels with virtually zero fossil carbon emission.

Cumulative corrosion loss – as measured over 32 years on bridges in Finland – demonstrates the superior corrosion resistance of SSAB Weathering steels.
Cell tower companies looking for durable corrosion resistance and lower embedded CO2 emissions in their masts can take advantage of SSAB Weathering steels’ galvanizing alternative. Another advantage: the muted presence of the patinated, weathered steel helps the telecom mast visually blend better into its surroundings.