Toolox® 40

The pre-hardened, exceptionally clean engineering and tool steel

Download data sheet

General Product Description

The pre-hardened, exceptionally clean engineering and tool steel.

Toolox® 40 is a pre-hardened steel suitable for engineering components and mold applications. It possesses good dimensional stability after machining.

Toolox® 40 features the same machinability as the conventional P20/W.Nr 1.2311 steel, despite its nearly 100 HBW higher nominal hardness, in combination with the renowned high dimensional stability of Toolox®. This makes Toolox® 40 your ideal choice in engineering components that require higher strength, or in molds and dies that demand higher wear resistance.

Dimension Range

Toolox® 40 is available as plates in thicknesses between 6.0 - 130.0 mm. Other dimensions can be available on request.

Mechanical Properties

Thickness
(mmin)
Thickness
(mmin)
6.0 - 130.00.236 - 5.118
Hardness 1)
(HBW)
360 - 420

1) Hardness is measured, according to EN ISO 6506-1, on a milled surface 0.5 - 2 mm below the plate surface.

Impact Properties

Thickness
(mmin)
Thickness
(mmin)
6.0 - 130.00.236 - 5.118
Min impact energy for transversal testing,
Charpy V 10x10 mm test specimen 1)
20 J / 20 °C15 ft-lbs / 68 °F

1) Impact testing according to EN 10 025, EN ISO 148 with a 2 mm striker.

Ultrasonic testing

Ultrasonic inspection is carried out according to: EN 10160 with extra demands according to specification SSAB V6.

Tolerances

More details are given in SSAB’s brochure Toolox® Guarantees and on www.ssab.com.

Thickness

Tolerances according to Toolox® Thickness Guarantee.

Toolox® Guarantees meets the requirements of EN 10029 Class C but offers more narrow tolerances.

Length and Width

Tolerances according to EN 10029.

Flatness

Tolerances are according to Toolox® Flatness Guarantees, which are more restrictive than EN 10029 Class N (steel type L).

Surface Properties

According to EN 10163-2 Class B, Subclass 3.

Delivery Conditions

Quenched and Tempered at a minimum temperature of 590 °C.

On delivery from SSAB, Toolox® material meet the following specifications:

  • Free from mill scale
  • Not repair welded

Delivery requirements can be found in SSAB’s brochure Toolox® Guarantees or at www.ssab.com.

Recommendations and instructions

pdf384 Kb

Toolox® in engineering applications

pdf1.34 Mb

Machining recommendations for Toolox®

Used for

  • Tooling & Engineering
  • High temperatures (up to 590°C)

Available standard

  • EN 10029

High-strength engineering tool steel

The new generation of tool steel.