COR-TEN® surface

SSAB COR-TEN® Steel in the grades and shapes you need

SSAB COR-TEN® portfolio includes a wide range of heavy plate, hot and cold rolled strip and tubes.

SSAB COR-TEN® steel powers your business

SSAB COR-TEN® steel from SSAB is easy to work with and give your buildings and products the long-term performance you are looking for.

SSAB COR-TEN® steel has excellent properties for forming, machining and welding. The SSAB COR-TEN® portfolio includes a wide range of grades with mechanical properties and dimensional tolerances that generally exceed the standards given by EN 10025-5, and ASTM grades.

Order SSAB COR-TEN® steel here

SSAB COR-TEN® steel grades are available from SSABs distributors. You can also order a trial delivery for testing in your production. 

Your local service contact will answer any questions about ordering.

Contact us
Product Name

SSAB COR-TEN® A, cold rolled

Dimensions
T: 0.50 - 3.00 mm
W: Up to 1530 mm
T: 0.020 - 0.118 in
W: Up to 60.24 in
Datasheet
Product Name

SSAB COR-TEN® A for façades

Dimensions
T: 0.50 - 3.00 mm
W: Up to 1530 mm
T: 0.020 - 0.118 in
W: Up to 60.24 in
Datasheet
Product Name

SSAB COR-TEN® A, hot rolled

Dimensions
T: 2.00 - 12.70 mm
W: Up to 3300 mm
T: 0.0787 - 0.5000 in
W: Up to 129.9 in
Datasheet
Product Name

SSAB COR-TEN® B

Dimensions
T: 2.00 - 40.00 mm
W: Up to 3300 mm
T: 0.0787 - 1.575 in
W: Up to 129.9 in
Datasheet
Product Name

SSAB COR-TEN® B-D

Dimensions
T: 2.00 - 40.00 mm
W: Up to 3300 mm
T: 0.0787 - 1.575 in
W: Up to 129.9 in
Datasheet
Product Name

SSAB COR-TEN B Tube

Dimensions
Circular: 48.3 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.5 mm
Circular: 1.90 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.492 in
Datasheet