Product offer and datasheets

SSAB Form Tubes

Product Name

SSAB Form Tube 220

Dimensions
Circular: 16 - 88.9 mm
Square: 19x19 - 70x70 mm
Rectangular: 25x15 - 100x40 mm
Flat oval: 25x15 - 78x38 mm
Oval: 22x16.5 - 31x17.5 mm
Wall Thickness: 0.9 - 3.0 mm
Circular: 0.63 - 3.50 in
Square: in
Rectangular: in
Flat oval: in
Oval: in
Wall Thickness: 0.04 - 0.12 in
Standards
EN 10305-3, EN 10305-5
Datasheet
Product Name

SSAB Form Tube 320

Dimensions
Circular: 16 - 88.9 mm
Square: 19x19 - 70x70 mm
Rectangular: 25x15 - 100x40 mm
Flat oval: 25x15 - 78x38 mm
Oval: 22x16.5 - 31x17.5 mm
Wall Thickness: 0.9 - 3.0 mm
Circular: 0.63 - 3.50 in
Square: in
Rectangular: in
Flat oval: in
Oval: in
Wall Thickness: 0.04 - 0.12 in
Standards
EN 10305-3, EN 10305-5
Datasheet
Product Name

SSAB Form Tube 420

Dimensions
Circular: 16 - 88.9 mm
Square: 19x19 - 70x70 mm
Rectangular: 25x15 - 100x40 mm
Wall Thickness: 0.9 - 3.0 mm
Circular: 0.63 - 3.50 in
Square: in
Rectangular: in
Wall Thickness: 0.04 - 0.12 in
Standards
EN 10305-3, EN 10305-5
Datasheet

SSAB Boron Tubes

Product Name

SSAB Boron Tube 22

Dimensions
Circular: 16 - 88.9 mm
Square: 19x19 - 70x70 mm
Rectangular: 25x15 - 100x40 mm
Wall Thickness: 0.9 - 3.0 mm
Circular: 0.63 - 3.50 in
Square: in
Rectangular: in
Wall Thickness: 0.04 - 0.12 in
Standards
EN 10305-3, EN 10305-5
Datasheet

Docol® Tubes

Product Family

Docol Tube 590DP

Product Family

Docol Tube 980DP

Product Name
CR750Y980T-DP
Dimensions
Circular: 28.0 - 60.0 mm
Square: 25x25 - 50x50 mm
Rectangular: 40x20 - 60x40 mm
Wall Thickness: 1.0 - 2.0 mm
Circular: 1.10 - 2.36 in
Square: in
Rectangular: in
Wall Thickness: 0.039 - 0.079 in
Standards
EN 10305-3, EN 10305-5, VDA 239-100
Datasheet
Product Family

Docol Tube 600LA

Product Name
HR600LA
Dimensions
Circular: 22.0 - 88.9 mm
Square: 30x30 - 60x60, 30x30 - 60x60 mm
Rectangular: 30x20 - 100x40 mm
Wall Thickness: 2.0 - 3.0 mm
Circular: 0.866 - 3.50 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.12 in
Standards
EN 10305-3, EN 10305-5
Datasheet
Product Family

Docol Tube 700LA

Product Name
HR700LA
Dimensions
Circular: 32.0 - 88.9 mm
Wall Thickness: 2.0 - 3.0 mm
Circular: 1.26 - 3.50 in
Wall Thickness: 0.079 - 0.12 in
Standards
EN 10305-3
Datasheet
Product Family

Docol Tube R8

Product Name
Docol Tube R8
Dimensions
Circular: 25.4 - 50.8 mm
Wall Thickness: 1.24 - 2.4 mm
Circular: 1.00 - 2.00 in
Wall Thickness: 0.0488 - 0.095 in
Standards
EN 10305-3
Datasheet