Consumable manufacturer/ Min yield strength MPa (ksi) 400 (58) 470 (68 540 (78) 610 (97) 680 (100) 745 (108)
AWS Class ER 7X* ER 8X” ER 9X” ER10X* ER11X” ER12X”
ELGA Elgacore DWA 51B, Elgacore DWA 50 Elgacore DWA 55L Elgacore DWA 65L   Elgacore R690  
ESAB Tubrod 15.00, Filarc PZ 6113S OK Tubrod 15.17 Dual-Shield 55, Dual-Shield CrMo2 Dual-Shield 62 Dual-Shield 69, OK Tubrod 15.27 Filarc PZ 6149
LINCOLN ELECTRIC Outershield 71E-H, Outershield 71MS-H Outershield 12-H, Outershield 19-H Outershield 20-H Outershield 101Ni-HSR Outershield 690-H  
BÖHLER Ti52-FD, Union TG 55 M Ti 60-FD, Ti 2 Ni T-FD Kb 65 T-FD   Kb 85 T-FD  
OERLIKON Fluxofil 14HD, Fluxofil 19HD Fluxofil 20, Fluxofil 20HD        

* X can stand for one or several code characters