Small size increase risk of softening

The smaller the piece that is thermally cut, the greater the risk of the whole component being softened. When small parts are cut, the heat supplied by the cutting torch and by preheating will accumulate in the workpiece. Consequently, the smaller the size of the cut part, the higher the risk of softening.

When oxy-fuel is used for cutting 30 mm (1.181”) or thicker plate, a rule of thumb applies: There is a risk of loss of hardness of the entire component if the distance between two cuts is less than 200 mm (7.874”). However, for thicknesses below 30 mm (1.181”), it is possible to cut smaller parts without loss of hardness.

A convenient method to determine if the piece is too small is to measure the temperature of the part directly after it has been cut out.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.