Customer satisfaction surges as Industrias Baco pioneers Hardox® 500 Tuf steel in tipper trucks
March 25, 2021 6 min read

Case details
Argentina’s leading tipper manufacturer, Industrias Baco, was the first company in Argentina to produce half-pipe tipper truck bodies made in Hardox® 500 Tuf wear plate. The results? More satisfied customers, stronger yet lighter bodies, and about a 30% longer product lifespan.
Industrias Baco is the market leader in Argentina in the heavy-duty tipper truck segment. The company has been producing tippers since 1953 and has helped transform the market for tipper trucks in the country with the help of Hardox® 500 Tuf.