How to machine > How to drill > Preparation

Preparation

Tool holders should be carefully selected.

Tool holders such as the morse taper are most often found in radial and pillar drilling machines. This type of attachment is not stable and is best suited for high-speed steel drills.

Morse taper.

Machines equipped with internal cooling and a backlash-free machine attachment provide the drill with good conditions for a long life. An example of tool attachment that can be used is a hydraulic chuck or a shrink chuck they will minimize tool runout.

Hydraulic chuck.

The tool run-out should not exceed 0,02 mm.

Tool run-out.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.