How does thermal cutting remove steel?
As the name suggests, thermal cutting uses thermal energy to cut steel. Depending on the source of this energy, there are several methods of thermal cutting. While the specific technologies vary, the fundamental principle is the same: the material is heated until it reaches a molten state and is then blown out of the cut zone using a jet of oxygen or another gas.