Tipper design > Tipper body design
U-shape tipper design considerations
In a U-shape design, sometimes called a half-pipe design, part or all of the body is rounded in the shape of a U.
The actual shape can vary, from a squarer cross section to a more rounded cross section. The corners of the body can be bent in various ways.
The main method of forming the corners is to use a press brake, which is more flexible and can bend a longer section than a roller bending machine. Because the U-shape does not have any corners and the load distribution is over the entire design, the stress is not centered. The risk of placing welds in high-stress areas is therefore lower with the U-shape design. Finally, because the U-shape lacks sharp corners, it usually has a longer service life.

U-shape tipper body design
The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products.
This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.