Tipper design > Manufacturing advantages of Hardox® wear steel in tipper bodies
Differences between mild steel and high-strength Hardox® wear steel
The illustration below shows an example of an upgrade from mild steel to Hardox® 450 and Strenx® 700 MC.
By minimizing the amount of stiffeners and using other methods of stiffening, like bending, the number of components was slashed from 50 to 19 parts. In addition, the weight savings resulting from this upgrade are 51 percent and the estimated emission savings are 3 tonnes (3.3 tons) CO2 per body.

Illustration of how a tipper made of mild steel (left) can be upgraded to a much more efficient one using high-strength steel (right).
In the graph below, the cost of the old version can be compared with the new version in high-strength steel. Although the initial material cost is higher for high-strength steel, its use in manufacturing brings both labor and cost savings. Both welding and cutting costs are lower than with the old design, which is typical since the thickness of a plate in high-strength steel can often be reduced. During cutting, the thinner the material is, the more easy and time-efficient the process.
In some cases, the manufacturing costs related to Hardox® steel are not lower. However, the lifespan of the product is also crucial to consider. By minimizing the number of parts, fewer welds and joints need to be used. Welds are often subject to fatigue and can thus decrease a product’s service life.

Example of relative production costs for an old design container vs. a new design container.
The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products.
This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.