Bucket design > Carbon footprint of buckets
Carbon footprint of a wheel loader bucket
This wheel loader bucket has been upgraded from Hardox® 450 to Hardox® 500 Tuf with improved design, making the bucket volume fit for an increased load capacity corresponding to the reduced bucket weight.

a) Previous design b) Upgraded design
Calculation data
Bucket model: Fronteq Eslöv Loader Bucket
Machine class: 35 tonne wheel loader
Diesel consumption, average: 40 litres/hour (assumption)
Machine usage per year: 4 000 hours/year
Design service lifetime: 3 years
Bucket volume: 11 m3 (SAE 1:2)
Weight of bucket (before upgrading): 7 256 kg
Weight of bucket (after upgrading): 6 286 kg (-970 kg or -13%)
Bucket payload capacity (before upgrading): 17 600 kg
Bucket capacity (after upgrading): 18 570 kg (+970 kg or +6%)
Carbon emission savings
Total lifetime CO2 savings: 77 tonnes (1.9 tonnes from less steel produced and 75 tonnes from higher load capacity)
Fuel reduction: 25 073 litres during lifetime (3 years). Corresponding to 40 116 EUR (at 1.6 EUR/litre).
CO2 payback time: 6 months.
Higher capacity in operation
If the extra capacity is used to run the loader machine more for higher revenue, assuming a masses moved revenue of 10 EUR/tonne, 4 000 tonnes moved per day and 330 days in operation per year:
Total profit increase: 740 873 EUR/year (with 72 750 tonnes extra massed moved per year).
The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products.
This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.