SSAB Laser® 460ML Plus

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

On this page

General Product Description

SSAB Laser® 460ML Plus is an advanced thermomechanically rolled weldable fine grain steel for laser cutting and cold forming. The SSAB guarantee for flatness, both before and after laser cutting, is ≤ 3 mm/m deviation.

SSAB Laser® 460ML Plus meets and exceeds the requirements of S460ML in EN 10025-4. Dual certification and CE marking are available upon request.

Dimension Range

Hide/Show specific columns Edit
Select columns to display
    Delivery form Thickness
    (mmin)
    Width
    (mmin)
    Length
    (mmin)
    SSAB Laser® 460ML Plus Hot rolled plate 10.0 - 25.00.394 - 0.984 1000 - 330039.37 - 129.9 2000 - 1500078.74 - 590.55
    Compare parameters

    Select one parameter to compare

    Comparison

      Mechanical Properties

      Hide/Show specific columns Edit
      Select columns to display
        Yield strength ReH
        (min MPa)
        Tensile strength Rm
        (MPa)
        Elongation A5
        (min %)
        Min. inner bending radius for a 90° bend 1)
        (x t)
        460 540 - 720 17 1.0
        Compare parameters

        Select one parameter to compare

        Comparison

          The mechanical properties are tested transverse to the direction of rolling.

          1) The bending guarantee is valid for both longitudinal and transverse direction.

          Impact Properties

          Hide/Show specific columns Edit
          Select columns to display
            Min. impact energy for longitudinal testing,
            Charpy V 10x10 mm test specimens
            40 J / -50 °C
            Compare parameters

            Select one parameter to compare

            Comparison

              Min. impact energy for longitudinal testing,
              Charpy V 10x10 mm test specimens
              40 J / -50 °C
              Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6mm. The specified minimum value corresponds to a full-size specimen.

              Chemical Composition (heat analysis)

              Hide/Show specific columns Edit
              Select columns to display
                C
                (max %)
                Si
                (max %)
                Mn
                (max %)
                P
                (max %)
                S
                (max %)
                CEV
                (max )
                0.13 0.03 1.6 0.020 0.015 0.39
                Compare parameters

                Select one parameter to compare

                Comparison

                  All SSAB Laser® steels are aluminum-killed (Al ≥ 0.015%) and grain-refined. Additionally, niobium (Nb), vanadium (V), titanium (Ti) and/or boron (B) may be used as single alloying element or in any combination.

                  Tolerances

                  All SSAB Laser® products are delivered with SSAB Laser® tolerances, which means increased guarantees compared to corresponding EN standards. Detailed information is available on ssab.com.

                  Thickness

                  SSAB Laser® tolerances correspond to 3/4 of EN 10029 as default.

                  Width

                  -0/+4-10mm depending on the thickness.

                  Length

                  Hide/Show specific columns Edit
                  Select columns to display
                    Nominal length
                    (mm)
                    Tolerance
                    (mm)
                    2000 ˂ l ≤ 10000 - 0 / + 15
                    10000 ˂ l ≤ 15000 - 0 / + 20
                    Compare parameters

                    Select one parameter to compare

                    Comparison

                      Nominal length
                      (mm)
                      2000 ˂ l ≤ 10000
                      Tolerance
                      (mm)
                      - 0 / + 15
                      Nominal length
                      (mm)
                      10000 ˂ l ≤ 15000
                      Tolerance
                      (mm)
                      - 0 / + 20

                      Shape

                      Tolerances according to EN 10029.

                      Flatness

                      ≤ 3 mm/m flatness deviation for both delivery condition and laser cut parts.

                      Surface Properties

                      According to EN 10163-2 Class A, Subclass 3.

                      Delivery Conditions

                      Thermomechanically rolled.

                      Surface and edge condition

                      Hot rolled plate: as rolled surface condition and cut edges as default.

                      Fabrication and Other Recommendations

                      All SSAB Laser® products have been optimized for laser cutting, cold forming and welding.

                      SSAB Laser® ML Plus products are thermomechanically rolled weldable fine grain steels for laser cutting and cold forming. It is not suited for heat treatments at temperatures above 580°C, since the material then may lose its guaranteed properties.

                      For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

                      Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

                      Contact Information

                      www.ssab.com/contact