SSAB Laser® 355ML Plus is an advanced thermomechanically rolled weldable fine grain steel for laser cutting and cold forming. The SSAB guarantee for flatness, both before and after laser cutting, is ≤ 3 mm/m deviation.
SSAB Laser® 355ML Plus meets and exceeds the requirements of S355ML in EN 10025-4. Dual certification and CE marking are available upon request.
SSAB Laser® 355ML Plus
The mechanical properties are tested transverse to the direction of rolling.
1) The bending guarantee is valid for both longitudinal and transverse direction.
All SSAB Laser® steels are aluminum-killed (Al ≥ 0.015%) and grain-refined. Additionally, niobium (Nb), vanadium (V), titanium (Ti) and/or boron (B) may be used as single alloying element or in any combination.
All SSAB Laser® products are delivered with SSAB Laser® tolerances, which means increased guarantees compared to corresponding EN standards. Detailed information is available on ssab.com.
SSAB Laser® tolerances correspond to 3/4 of EN 10029 as default.
-0/+4-10mm depending on the thickness.
Tolerances according to EN 10029.
≤ 3 mm/m flatness deviation for both delivery condition and laser cut parts.
According to EN 10163-2 Class A, Subclass 3.
Thermomechanically rolled.
All SSAB Laser® products have been optimized for laser cutting, cold forming and welding.
SSAB Laser® ML Plus products are thermomechanically rolled weldable fine grain steels for laser cutting and cold forming. It is not suited for heat treatments at temperatures above 580°C, since the material then may lose its guaranteed properties.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.