SSAB Form 200 is a mild steel intended for forming with the best conceivable properties in both drawing and stretch forming operations. SSAB Form 200 is used for a wide variety of applications including vehicle parts, refrigerators, electric radiators and water radiators.
SSAB Form 200 cold rolled meets and exceeds the requirements of DC01 in EN 10130.
SSAB Form 200 is available in thicknesses of 0.40-3.00 mm and widths up to 1500 mm as coils, slit coils and as cut to length in lengths up to 8.5 meters.
Yield strength Rp0.2 (max MPa) | Tensile strength Rm (MPa) | Elongation A80 1) (min %) |
|---|---|---|
260 | 280 - 380 | 29 |
The mechanical properties are tested in the transversal direction.
1) When the thickness is less than or equal to 0.7 mm and greater than 0.5 mm, the minimum value for elongation is reduced by 2 units. For a thickness less than or equal to 0.5 mm, the minimum value is reduced by 4 units.
C (max %) | Si (max %) | Mn (max %) | P (max %) | S (max %) | Al (min %) | Nb+Ti (max %) |
|---|---|---|---|---|---|---|
0.10 | 0.040 | 0.40 | 0.030 | 0.030 | 0.015 | 0.040 |
SSAB Form cold rolled products are supplied with tolerances in accordance to EN 10131. More narrow thickness tolerances according to the SSAB standard are available upon request.
Cold rolled.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.