SSAB Domex 460LA is a high-strength, low-alloy steel intended for general presswork, bending and forming. SSAB Domex 460LA offers consistent properties that assist modern, rapid production methods.
SSAB Domex 460LA meets and exceeds the requirements of HC460LA in EN 10268.
SSAB Domex 460LA is available in thicknesses of 0.50-1.60 mm and widths up to 1500 mm as coils, slit coils and as cut to length in lengths up to 8.5 meters.
Yield strength ReL (MPa) | Tensile strength Rm (MPa) | Elongation A80 1) (min %) | Min. inner bending radius for a 90° bend 2) (x t) |
|---|---|---|---|
460 - 580 | 510 - 660 | 13 | 0.5 |
The mechanical properties are tested in the transversal direction.
Bending properties for both longitudinal and transversal direction.
1) When the thickness is less than or equal to 0.7 mm and greater than 0.5 mm, the minimum value for elongation is reduced by 2 units. For a thickness less than or equal to 0.5 mm, the minimum value is reduced by 4 units.
2) t = Sheet thickness.
C (max %) | Si (max %) | Mn (max %) | P (max %) | S (max %) | Al (min %) | Nb+Ti (max %) |
|---|---|---|---|---|---|---|
0.10 | 0.60 | 1.50 | 0.030 | 0.025 | 0.015 | 0.10 |
SSAB Domex LA products are supplied with thickness, width and length tolerances in accordance to EN 10131. Narrower tolerances are available upon request.
Cold Rolled.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.