Duroxite® 300 Wire

Download data sheet

General Product Description

Duroxite® 300 Wire is a flux-cored welding wire for hardfacing components subject to extremely severe sliding wear applications using an open-arc or gas shielded arc welding processes. The weld deposit of Duroxite® 300 Wire consists of specially formulated abrasive materials employing a uniform glass-forming melt chemistry that allows high undercooling to be achieved. Duroxite® 300 weld overlay contains a unique high volume of ultra-fine tungsten-niobium-molybdenum-rich complex borocarbide phase with a grain size refined down to 500 nm. The borocarbides are completely wetted in a ductile matrix preventing premature pull-out delamination, crack nucleation and bridging. This results in a product with significantly improved service life that maintains high toughness in severe sliding wear applications.

Duroxite® 300 Wire is suitable for single or double-layer deposit with both stringer and oscillation beads. It naturally reveals stress-relief cracks after welding. Preheating, inter-pass temperature, and post-weld heat treatment are as needed according to the base metal recommendations. If welding fume generation is a concern, a gas shielded arc welding process is recommended. A slight drag angle is preferred for better performance while welding. If welding with downhill or uphill positions, reduced wire feed speed and voltage are preferred. Duroxite® 300 Wire is designed to weld on carbon steel or low alloy steel substrates experiencing severe wear for both dry and wet (slurry) abrasive environments at ambient or elevated temperatures up to 600°C (1100°F). Duroxite® 300 Wire is not compatible with austenitic alloys. Duroxite® 300 Wire is an excellent alternative to tungsten carbide hardfacing wire.

Key Benefits

  • Extreme wear resistance in dry and wet abrasive environments with a high degree of toughness.
  • Cost effective alternative to tungsten carbide wire with equivalent service life and better impact resistance.
  • Maintains a consistent wear resistance from surface down to 75% of the overlay.
  • Has uniform through-thickness hardness of 67 to 70 HRC for single and double-layer overlay.
  • Thinner thickness overlay applied compared to traditional chromium carbide overlay (CCO) or complex carbide overlay which result in a lighter weight product while increasing service life.

Typical Applications

Duroxite® 300 Wire is mainly designed to use for hardfacing any steel substrates (not compatible with austenitic alloys) undergoing extremely severe wear in mining, power generation, cement, oil sand, steel production, waste handling, and pulp and paper industries. Typical examples include:

Mining

Crusher rolls, Skip liners, Slurry pipes, Slurry pumps, Conveyor chains, Excavator bucket liners

Cement

Fan blades, Deflector blades, Cranker crushers

Oil sands

Surge bins, Feed chutes, Slurry pipes, Slurry pumps

Steel

Ore chutes

Power

Screw augers, Wear liner plates, Ash handling equipment liners

Agriculture

Grain shredding hammers, Sugar mill knives, Row crop sweeps

Oil and Gas

Fracking blender pumps

Construction

Snow plow shoes, Demolition tools

Standard Dimensions

Standard diameter
Metric
Standard diameter
Metric
1.6 mm

Mechanical Properties

Number of overlay passes
Number of overlay passes
Single pass
ASTM G65 – Procedure A weight loss 2)
Surface
(g max)
0.10
ASTM G65 – Procedure A weight loss 2)
75 % depth of overlay 3)
(g max)
0.10
Typical weld metal surface hardness
Weld deposit on mild steel 1)
(HRC)
67 - 70
Slurry jet erosion weight loss 4)
20o Impingement angle
(g typical)
0.0329
Slurry jet erosion weight loss 4)
45o Impingement angle
(g typical)
0.0591
Number of overlay passes
Number of overlay passes
Double passes
ASTM G65 – Procedure A weight loss 2)
Surface
(g max)
0.10
ASTM G65 – Procedure A weight loss 2)
75 % depth of overlay 3)
(g max)
0.10
Typical weld metal surface hardness
Weld deposit on mild steel 1)
(HRC)
67 - 70
Slurry jet erosion weight loss 4)
20o Impingement angle
(g typical)
0.0329
Slurry jet erosion weight loss 4)
45o Impingement angle
(g typical)
0.0591

1) Surface hardness is measured on machined flat surface just below overlay surface.

2) ASTM G65 is a standard test measuring sliding abrasion resistance using a dry sand/rubber wheel apparatus. ASTM G65-Procedure A is the most severe test method.

3) ASTM G65 wear test is conducted at 75% depth of the overlay materials to ensure consistently good wear resistance from the top surface through to the depth of 75% of the overlay.

4) Duroxite 300 outperforms typical CCO in an SJE test. Typical CCO loses 0.0689 g at 20° and 0.0995 g at 45° impingement angles in the same test. For more information about Duroxite® 300 and its performance in a Slurry Jet Erosion Test, please see the Duroxite® Brochure – The Latest in Overlay Technology available at ssab.com.

Test results for mechanical properties

Test results for mechanical properties, deposit overlay chemical composition, surface hardness, and ASTM G65-A weight loss were obtained from a weld produced and tested according to prescribed standards, and should not be assumed to be the expected results in a particular application or weldment. Actual results will vary depending on many factors, including, but not limited to, weld procedure, substrate chemistry and working temperature, weldment design and fabrication methods. Users are cautioned to confirm by qualification testing, or other appropriate means, the suitability of any welding consumable and procedure before use in the intended applications.

Chemical Composition

Typical weld deposit chemical composition (wt. %)
C
Typical weld deposit chemical composition (wt. %)
C
< 5.0
Typical weld deposit chemical composition (wt. %)
Mn
< 5.0
Typical weld deposit chemical composition (wt. %)
Si
< 2.0
Typical weld deposit chemical composition (wt. %)
Cr
< 20.0
Typical weld deposit chemical composition (wt. %)
W
< 10.0
Typical weld deposit chemical composition (wt. %)
B
< 5.0
Typical weld deposit chemical composition (wt. %)
Mo
< 10.0
Typical weld deposit chemical composition (wt. %)
Nb
< 10.0
Typical weld deposit chemical composition (wt. %)
Al
< 5.0
Typical weld deposit chemical composition (wt. %)
Fe
Balance

Welding recommendations

Welding conditions
Current type
Welding conditions
Current type
DCEP (Direct current electrode positive)
Welding conditions
Shielding gas
Open arc (no shielding)
Welding conditions
Welding positions
Flat, horizontal, half up, half down
Welding conditions
Current type
Welding conditions
Current type
DCEP (Direct current electrode positive)
Welding conditions
Shielding gas
75% Ar / 25% CO2
98% Ar / 2% O2
Welding conditions
Welding positions
Flat, horizontal, half up, half down

Welding parameters recommendations

Shielding
Shielding
Open arc (no shielding)
Diameter
1.6 mm0.06250 mm
Amperage (A)
220
Voltage (V)
24 - 25
Wire feed speed
7.0 m/min
Stick-out
25 mm
Shielding
Shielding
Gas shielded
Diameter
1.6 mm0.06250 mm
Amperage (A)
220
Voltage (V)
24 - 25
Wire feed speed
7.0 m/min
Stick-out
20 mm

Recovery: 90%

Delivery Conditions

Standard package
Type
Standard package
Type
Spool
Diameter
Metric
1.6 mm0.06250 mm
Weight
Metric
15 kg

Fabrication and Other Recommendations

The welded overlay components can be processed by welding, cutting, forming and machining. Specific recommendations can be found in the Duroxite® Product brochure or by consulting your local technical support representative.