Docol® 500LA high strength low alloy
More about high strength low alloy steelDownload data sheet
Download data sheet
The Docol 500LA steels are high-strength low-alloy steels that offer consistent properties for modern, rapid production methods. Typical applications include bent profiles. Docol HR500LA-UC can after agreement be adapted and delivered as dual certified with S500MC according to EN 10149-2.
Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm.
Slit strip and cut to length sheets are available upon request.
Grade and coating specific restrictions on available dimensions may occur.
1) A80 value applies for thicknesses < 3.00 mm.
2) A5 value applies for thicknesses ≥ 3.00 mm.
Hot rolled (UC): Tolerances in accordance to EN 10051.
Customized dimensional and shape tolerances are available upon request.
Uncoated (UC): available as oiled.
All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.