COR-TEN® portfolio includes a wide range of heavy plate, hot and cold rolled strip and tubes.
COR-TEN® steel grades are available from SSABs distributors. You can also order a trial delivery for testing in your production.
Your local service contact will answer any questions about ordering.
Contact usProduct Name | Dimensions | Datasheet |
---|---|---|
COR-TEN® A, cold rolled | T: 0.50 - 3.00 mm W: Up to 1530 mmT: 0.020 - 0.118 in W: Up to 60.24 in | |
COR-TEN® A for façades | T: 0.50 - 3.00 mm W: Up to 1530 mmT: 0.020 - 0.118 in W: Up to 60.24 in | |
COR-TEN® A, hot rolled | T: 2.00 - 12.70 mm W: Up to 3300 mmT: 0.0787 - 0.5000 in W: Up to 129.9 in | |
COR-TEN® B | T: 2.00 - 40.00 mm W: Up to 3300 mmT: 0.0787 - 1.575 in W: Up to 129.9 in | |
COR-TEN® B-D | T: 2.00 - 40.00 mm W: Up to 3300 mmT: 0.0787 - 1.575 in W: Up to 129.9 in |
COR-TEN® A, cold rolled
COR-TEN® A for façades
COR-TEN® A, hot rolled
COR-TEN® B
COR-TEN® B-D
Product Name | Dimensions | Datasheet |
---|---|---|
COR-TEN B Tube | Circular: 42.4 - 323.9 mm Square: 40x40 - 300x300 mm Rectangular: 50x30 - 400x200 mm Wall Thickness: 2.0 - 12.5 mmCircular: 1.67 - 12.75 in Square: in Rectangular: in Wall Thickness: 0.079 - 0.492 in |
COR-TEN B Tube