GreenCoat RWS Pural
Download data sheet
Download data sheet
GreenCoat RWS Pural color coated steel is available in regular finish and offers a wide range of colors inspired by Nordic nature.
GreenCoat RWS Pural offers the highest level of durability for rainwater systems using a double-sided coating (same coating is applied on both sides of the sheet).
GreenCoat RWS Pural color coated steel provides excellent corrosion resistance (RC5), gloss retention and color fastness (Ruv4). GreenCoat RWS Pural possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.
Excellent weather resistance together with regular maintenance and the cleaning of rainwater systems can maximize the service life of the product.
GreenCoat RWS Pural complies with current REACH regulations and is fully chromate-free.
SSAB’s color coated steels are all manufactured according to EN 10169.
GreenCoat and Pural are trademarks of the SSAB group of companies.
1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.
2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.
3) FAX fulfills the requirements of EN 10346 DX51D, DX52D/RWS fulfills the requirements of EN 10346 DX52D.
Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.
Colors
GreenCoat RWS Pural
Winter White
RR20 / SS0005
Pebble Grey
RR21 / SS0011
Stone Grey
RR22 / SS0554
Mountain Grey
RR23 / SS0036
Nordic Night Black
RR33 / SS0015
Walnut Brown
RR32 / SS0387
Chestnut Brown
RR887 / SS0435
Cottage Red
RR29 / SS0758
Pine Green
RR11 / SS0830
Same coating is applied on both sides of the sheet.
The technical properties apply for both sides. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.
Reverse side stamping is not applicable for double sided products.