On this page
1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.
2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.
3) FAX fulfills the requirements of EN 10346 DX51D, PLX fulfills the requirements of EN 10346 DX54D.
Below are the colors currently available. Other colors can be agreed upon separately.
Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.
The product may have slight tonal difference between batches and especially if their time of production differs significantly.
Same coating is applied on both sides of the sheet.
The technical properties apply for both sides. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.