SSAB Virsbolt face plate

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

On this page

General Product Description

SSAB Virsbolt face plates are used with Virsbolt expandable rock bolts.

SSAB Virsbolt face plates are used to create a local surface support around the borehole where the Virsbolt expandable rock bolts are installed. The face plates are used to transfer the displacement of the rock mass into the rock bolt. SSAB Virsbolt face plates are used for tunneling, construction and mining.

Advantages using SSAB Virsbolt:

  • Provides immediate and full support action
  • Accommodates large rock movements and still maintain its high load bearing capacity
  • High deformability to accommodate ground movements in tension as well as in shear
  • Technical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Product Description Grade
      ASTM F432
      Typical load capacity (kN),
      not guaranteed
      Plate dimension
      (mmin x mmin)
      Hole dimension
      (mmin)
      Thickness
      (mmin)
      Weight
      (kg)
      Dome plate adjustable 120 Flexible plate for 120kN bolts, with an attachment hole N/A 50 150x1505.906x5.906 29x39 (Oval)1.142x1.535 (Oval) 40.157 Oiled: 0.67
      Plastic coated: 0.71
      Dome plate adjustable 160/240 Flexible plate for 160kN and 240kN bolts, with an attachment hole N/A 50 150x1505.906x5.906 39x44 (Oval)1.535x1.732 (Oval) 40.157 Oiled: 0.66
      Plastic coated: 0.70
      Dome plate 120 Plate for 120kN bolts 2 100 152x1525.984x5.984 30 (Round)1.181 (Round) 60.236 Oiled: 1.04
      Plastic coated: 1.08
      Dome plate 160/240 Plate for 160kN and 240kN bolts 3 140 152x1525.984x5.984 40 (Round)1.575 (Round) 60.236 Oiled: 1.01
      Plastic coated: 1.05
      Compare parameters

      Select one parameter to compare

      Comparison

        Tolerances

        Tolerances according to SSAB specifications.

        Please contact your local sales person for more information regarding tolerances.

        Delivery Conditions

        Oiled/ plastic coated. Delivery requirements can be found in SSAB’s brochure SSAB Virsbolt, expandable rock bolt for rock reinforcement or at www.ssab.com.