Tipper design > Dent resistance in tipper bodies
Rock weight
How should the body be designed if it needs to handle blasted rocks from a primary crusher or secondary crusher?
To understand the answer, we need to know something about the rocks’ weight. This is not straightforward because rocks have different complex shapes, and different mineral compositions with varying densities. However, the weight of a rock increases significantly as its diameter increases, as shown in the table below.

The rock size defines the crusher gap: a) Minimum crusher gap. b) Maximum crusher gap.
Typical stone sizes and weights for blasted and crushed rock.
Typically a dump body is loaded with a mix of rocks, sand, clay and water and contains voids, so the rock density is not directly proportional to the volume of the body. A typical density for crushed aggregate is around 1600 - 1800 kg/m3 (100 – 112 lb/ft3) and the density of granite is 2520 - 2810 kg/m3 (157 - 175 lb/ft3). Because the largest rocks are the ones that cause dents, the rock density is worthwhile considering. Other properties, such as toughness, will also play an important role in dent resistance.
Weight of granite rock of different sizes.
The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products.
This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.