Toolox® 44

The pre-hardened steel for extrusion dies and engineering components

Contact us

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

On this page

General Product Description

Toolox® 44 is a steel already heat treated to the final properties.Thus saving time, costs and risks associated with heat treatment.

The very high strength is combined with a high and guaranteed toughness as well as an excellent fatigue resistence. Making Toolox® 44 the ideal choice for the most demanding engineering and mould and die applications.

Toolox® 44 can be surface hardened with methods like nitriding, laser and induction. Giving the possibilities to even further improve the performance.

Dimension Range

Toolox® 44 is available as plates in thicknesses between 6.0 - 130.0 mm. Other dimensions can be available on request.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Thickness
    (mmin)
    Hardness 1)
    (HBW)
    Yield strength Rp0.2
    (min MPaksi)
    Tensile strength Rm
    (min MPaksi)
    Elongation A5
    (min %)
    6.0 - 130.00.236 - 5.118 410 - 475 1150166 1300188 8
    Compare parameters

    Select one parameter to compare

    Comparison

      1) Hardness is measured, according to EN ISO 6506-1, on a milled surface 0.5 - 2 mm below the plate surface.

      Impact Properties

      Hide/Show specific columns Edit
      Select columns to display
        Thickness
        (mmin)
        Min impact energy for transversal testing,
        Charpy V 10x10 mm test specimen 1)
        6.0 - 130.00.236 - 5.118 18 J / 20 °C15 ft-lbs / 64 °F
        Compare parameters

        Select one parameter to compare

        Comparison

          Thickness
          (mmin)
          6.0 - 130.00.236 - 5.118
          Min impact energy for transversal testing,
          Charpy V 10x10 mm test specimen 1)
          18 J / 20 °C15 ft-lbs / 64 °F

          1) Unless otherwise agreed, transverse impact testing according to EN 10025-6 option 30 will apply. For thicknesses between 6 - 11.9 mm, sub-size Charpy V-specimens are used. The specified minimum value is then proportrional to the cross-sectional area of the specimen compared to a full-size specimen (10 x 10 mm).

           

           

           

          Ultrasonic testing

          Ultrasonic inspection is carried out according to : EN 10 160 with extra demands according to specification SSAB V6.

          Tolerances

          More details are given in SSAB’s brochure Toolox® Guarantees and on www.toolox.com.

          Thickness

          Tolerances according to Toolox® Thickness Guarantee.

          Toolox® Guarantees meets the requirements of EN 10029 Class C but offers more narrow tolerances.

          Length and Width

          Tolerances according to EN 10029.

          Flatness

          Tolerances are according to Toolox® Flatness Guarantees, which are more restrictive than EN 10029 Class N (steel type L).

          Surface Properties

          According to EN 10163-2 Class B, Subclass 3.

          Delivery Conditions

          Quenched and Tempered at a minimum temperature of 590 °C.

          On delivery from SSAB the plates meet the following specifications:

          • Free from mill scale
          • Not repair welded

          Delivery requirements can be found in SSAB’s brochure Toolox® Guarantees or at www.toolox.com.

          Recommendations and instructions

          pdf 384 Kb
          Toolox® in engineering applications
          pdf 1.34 Mb
          Machining recommendations for Toolox®

          Used for

          • Tooling & Engineering
          • High temperatures (up to 590°C)

          Available standard

          • EN 10029

          High-strength engineering tool steel

          The new generation of tool steel.