General Product Description

SSAB Laser® 460MC Plus is an advanced high yield strength cold forming steel for laser cutting. The SSAB guarantee for flatness, both before and after laser cutting, is ≤ 3 mm/m deviation.

SSAB Laser® 460MC Plus meets and exceeds the requirements of S460MC in EN 10149-2. Upon agreement, it can be delivered as dual certified. This dual certification will enable producers of steel structures, in accordance with EN 1090, to use SSAB Laser® 460MC Plus in their CE-marked final component or structure.

Dimension Range

Hide/Show specific columns Edit
Select columns to display
    Delivery form Thickness
    (mmin)
    Width
    (mmin)
    Length
    (mmin)
    Hot rolled sheet as rolled 3.0 - 12.00.12 - 0.472 1000 - 180039.37 - 70.87 1000 - 1600039.37 - 629.92
    Hot rolled sheet pickled and oiled 2.0 - 8.00.079 - 0.31 1000 - 160039.37 - 62.99 1000 - 1600039.37 - 629.92
    Compare parameters

    Select one parameter to compare

    Comparison

      Mechanical Properties

      Hide/Show specific columns Edit
      Select columns to display
        Yield strength ReH
        (min MPa)
        Tensile strength Rm
        (MPa)
        Elongation A80 1)
        (min %)
        Elongation A5 2)
        (min %)
        Min. inner bending radius for a 90° bend 3)
        (x t)
        460 520 - 670 14 19 0.0
        Compare parameters

        Select one parameter to compare

        Comparison

          The mechanical properties are tested in the longitudinal direction.

          1) A80 value applies for thicknesses < 3.00 mm.

          2) A5 value applies for thicknesses ≥ 3.00 mm.

          3) The bending guarantee is valid for both longitudinal and transverse direction.

          Impact Properties

          Hide/Show specific columns Edit
          Select columns to display
            Min. impact energy for longitudinal testing,
            Charpy V 10x10 mm test specimens
            40 J / -60 °C
            Compare parameters

            Select one parameter to compare

            Comparison

              Min. impact energy for longitudinal testing,
              Charpy V 10x10 mm test specimens
              40 J / -60 °C
              Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6mm. The specified minimum value corresponds to a full-size specimen.

              Chemical Composition (ladle analysis)

              Hide/Show specific columns Edit
              Select columns to display
                C
                (max %)
                Si
                (max %)
                Mn
                (max %)
                P
                (max %)
                S
                (max %)
                CEV
                (max )
                0.12 0.03 1.6 0.020 0.015 0.39
                Compare parameters

                Select one parameter to compare

                Comparison

                  All SSAB Laser® steels are aluminum-killed (Al ≥ 0.015%) and grain-refined. Additionally, niobium (Nb), vanadium (V), titanium (Ti) and/or boron (B) may be used as single alloying element or in any combination.

                  Tolerances

                  All SSAB Laser® products are delivered with SSAB Laser® tolerances, which means increased guarantees compared to corresponding EN standards. Detailed information is available on ssab.com.

                  Thickness

                  Hot rolled sheet: SSAB Laser® tolerances correspond to ⅔ of EN 10051 as default. Tighter tolerances are available upon request.

                  Width

                  Hot rolled sheet: -0/+20 mm for mill edge sheet; -0/+2 mm for cut edge sheet. Tighter tolerances are available upon request.

                  Length

                  Hide/Show specific columns Edit
                  Select columns to display
                    Nominal length
                    (mm)
                    Tolerance
                    (mmin)
                    l ≤ 4000 - 0 / + 3- 0 / + 0.1
                    4000 ˂ l ≤ 6000 - 0 / + 4- 0 / + 0.2
                    6000 ˂ l ≤ 8000 - 0 / + 5- 0 / + 0.2
                    8000 ˂ l ≤ 13000 - 0 / + 6- 0 / + 0.2
                    13000 ˂ l ≤ 16000 - 0 / + 8- 0 / + 0.3
                    Compare parameters

                    Select one parameter to compare

                    Comparison

                      Nominal length
                      (mm)
                      l ≤ 4000
                      Tolerance
                      (mmin)
                      - 0 / + 3- 0 / + 0.1
                      Nominal length
                      (mm)
                      4000 ˂ l ≤ 6000
                      Tolerance
                      (mmin)
                      - 0 / + 4- 0 / + 0.2
                      Nominal length
                      (mm)
                      6000 ˂ l ≤ 8000
                      Tolerance
                      (mmin)
                      - 0 / + 5- 0 / + 0.2
                      Nominal length
                      (mm)
                      8000 ˂ l ≤ 13000
                      Tolerance
                      (mmin)
                      - 0 / + 6- 0 / + 0.2
                      Nominal length
                      (mm)
                      13000 ˂ l ≤ 16000
                      Tolerance
                      (mmin)
                      - 0 / + 8- 0 / + 0.3

                      Shape

                      Tolerances according to EN 10051.

                      Flatness

                      ≤ 3 mm/m flatness deviation for both delivery condition and laser cut parts.

                      Surface Properties

                      According to EN 10163-2 Class B, Subclass 3.

                      Delivery Conditions

                      Thermomechanically rolled.

                      Surface and edge condition

                      SSAB Laser® MC Plus products are available in as rolled or pickled and oiled surface condition with mill edge. Cut edge sheets are available upon request.

                      Fabrication and Other Recommendations

                      All SSAB Laser® products have been optimized for laser cutting, cold forming and welding.

                      SSAB Laser® MC Plus products are cold forming steels not suited for heat treatments at temperatures above 580°C, since the material then may lose its guaranteed properties.

                      For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

                      Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.